Trace amount of taurine leveling agent for stable Zn anode DOI Creative Commons
Xin Zhang, Kai Zheng, Dengwei Hu

и другие.

RSC Advances, Год журнала: 2024, Номер 14(54), С. 40247 - 40254

Опубликована: Янв. 1, 2024

The study introduces a trace amount of taurine (TAU) as leveling additive into the electrolyte to optimize microstructure and anode interface chemistry, which can achieve highly reversible zinc deposition dissolution.

Язык: Английский

Preformation of Zn based layered double hydroxides on Zn powder solvent-free electrode for low temperature soft-package Zn-MnO2 battery DOI
Jianchun Wu, Zhiyong Liu, Haitao Zhou

и другие.

Journal of Power Sources, Год журнала: 2025, Номер 640, С. 236778 - 236778

Опубликована: Март 16, 2025

Язык: Английский

Процитировано

0

Perinone with fast proton insertion chemistry for durable aqueous zinc battery DOI

Yixiao Yang,

Qing Lang,

Jian Zhang

и другие.

Chemical Engineering Journal, Год журнала: 2025, Номер unknown, С. 161650 - 161650

Опубликована: Март 1, 2025

Язык: Английский

Процитировано

0

The Europium-Based Artificial Solid Electrolyte Interphase for High-Performance Aqueous Zinc-Ion Batteries DOI
Xiaowei Zhao,

Mengyu Liu,

Ruixin Zhang

и другие.

ACS Applied Polymer Materials, Год журнала: 2025, Номер unknown

Опубликована: Март 20, 2025

Язык: Английский

Процитировано

0

Sacrificial reduction effects derived inorganic-rich hybrid solid electrolyte interfaces for long-term and high reversibility aqueous zinc-ion batteries DOI
Yu Chen,

Jiahong Fan,

Qian Li

и другие.

Chemical Engineering Journal, Год журнала: 2025, Номер unknown, С. 161858 - 161858

Опубликована: Март 1, 2025

Язык: Английский

Процитировано

0

In-situ hybrid armor layer enabled by additive-anion synergy for dendrite-free and stable Zn anode DOI
Han Yu, Yufei Xue, Teng Wang

и другие.

Chemical Engineering Journal, Год журнала: 2025, Номер unknown, С. 161917 - 161917

Опубликована: Март 1, 2025

Язык: Английский

Процитировано

0

High-Stability Zinc Anodes Modulated by Solvation Structure and Interface Chemistry Toward Printable Zinc-Ion Capacitors DOI
Quancai Li,

Weinan Tang,

Guilin Tang

и другие.

Energy storage materials, Год журнала: 2025, Номер unknown, С. 104214 - 104214

Опубликована: Март 1, 2025

Язык: Английский

Процитировано

0

Synergistic Gradient Design of a Sandwich‐Structured Heterogeneous Anode for Improved Stability in Aqueous Zinc‐Ion Batteries DOI
Zhuo Wang,

Jiabao Dong,

Kexin Zhang

и другие.

Advanced Functional Materials, Год журнала: 2025, Номер unknown

Опубликована: Апрель 8, 2025

Abstract Aqueous Zn‐ion batteries provide a low‐cost energy storage solution but face challenges such as dendrite formation and interface instability, which become more pronounced at high currents capacities. Herein, scalable sandwich‐structured heterogeneous anode is proposed for aqueous zinc that integrate three functionally synergistic layers. A robust 3D ZnO@C substrate (from calcined Bio‐MOF‐100, BMC) with dense nucleation sites guides orderly Zn deposition, while controllable pre‐deposited intermediate layer precisely regulates 2 ⁺ flux. An artificial indium‐based protective top‐layer chemically isolates the active from electrolyte, effectively suppresses interfacial corrosion, enhances interlayer contact to minimize impedance maintaining structural integrity during cycling. The synergies endow symmetric cell an ultra‐long cycle life exceeding 2000 h stable plating/stripping remarkable depth of discharge (76%) under current/areal capacity conditions (6 mA cm −2 /12 mAh ). Additionally, BMC@Zn@In//(NH 4 ) V 10 O 25 ·8H full battery achieves lifespan 5000 cycles, BMC@Zn@In//activated carbon hybrid supercapacitor demonstrates impressive 16 000 cycles. This study identifies mechanism ultra‐stable promising applications in batteries.

Язык: Английский

Процитировано

0

ZnNCN protective layer with high zincphilicity and ionic conductivity for stable zinc metal anodes DOI

Yaoyong Dong,

Fangzhong Liu,

Ting Song

и другие.

Chemical Engineering Journal, Год журнала: 2025, Номер unknown, С. 162630 - 162630

Опубликована: Апрель 1, 2025

Язык: Английский

Процитировано

0

Engineering Artificial Protrusions of Zn Anodes for Aqueous Zinc Batteries DOI
Jifei Sun,

Xinhua Zheng,

Zhengxin Zhu

и другие.

Nano Letters, Год журнала: 2025, Номер unknown

Опубликована: Апрель 21, 2025

Uncontrollable dendrite growth can jeopardize the cycle life of aqueous Zn batteries. Here, we propose a general strategy engineering artificial protrusions (APs) on electrode surface to regulate distribution interface electric field and induce stable plating/stripping for The junction-free AP-Cu network is constructed Cu foil by an ultrafast Joule-heating-welding method. COMSOL simulation reveals that stronger microelectric formed around individual AP, which effectively uniform nucleation network. Guided structural advantages AP design, AP-Cu∥Zn cell delivers average Coulombic efficiency (CE) 99.85% at 2 C with areal capacity 1.77 mAh cm-2 over 3000 cycles. Moreover, design enables cycling both Zn|AP-Cu∥V2O5 anode-free AP-Cu∥Br2 full cells, providing promising development high-performance energy storage devices.

Язык: Английский

Процитировано

0

Rational Design of a Bilayer Interface for Long‐Term Stability of Zn Anodes and MnO2 Cathodes DOI

Kaiping Zhu,

Wubin Zhuang,

Nanyang Wang

и другие.

Advanced Materials, Год журнала: 2025, Номер unknown

Опубликована: Апрель 28, 2025

Abstract Understanding the composition–characteristics–performance relationship of electrolyte–electric double layer–electrode–electrolyte interface (EEI) is crucial to construct stable EEIs for high‐performance aqueous Zn–MnO 2 batteries (AZMBs). However, interaction mechanisms in AZMBs remain unclear. This work introduces sodium thioctate (ST) into ZnSO 4 electrolyte a bilayer EEI on both Zn and MnO electrodes. First, zincophilic ST regulates solvation structure hydrated 2+ , suppressing corrosion hydrogen evolution reaction. Second, specific adsorption reconstructs inner Helmholtz plane, facilitating desolvation homogenizing charge distribution. Finally, molecules undergo reversible polymerization at interface, forming with poly(zinc thioctate) outer layer ZnS–organic amorphous layer, which ensures uniform zinc‐ion flux enhances mechanical stability. Additionally, dynamic disulfide bonds further enable self‐regulation self‐healing mitigating damage during cycling. As result, ST‐enhanced symmetric battery achieves 7800 cycles 60 mA cm −2 while AZMB exhibits only 0.0014% capacity decay over 10 000 2000 g −1 . engineering strategy offers effective guidance rational design safe long‐life batteries.

Язык: Английский

Процитировано

0