SiO2/polydopamine photothermal superhydrophobic coating with good anti-icing performance DOI
Yuting Zhong, Yong Liu,

Xiangming Yang

et al.

Surface Engineering, Journal Year: 2024, Volume and Issue: 40(7-8), P. 907 - 916

Published: July 1, 2024

The icing phenomenon has become a safety hazard for the normal operation of equipment. In this work, we report strategy simply obtaining photothermal anti-icing coatings by spraying acrylic resin, polydimethylsiloxane and polydopamine modified SiO 2 particles on steel plate substrate. prepared icephobic AR/PDMS/SiO @PDA composite coating not only excellent superhydrophobicity (WCA = 162°). It also shows good anti- de-icing performances. superhydrophobic surface was able to delay freezing 614 s at −20°C, ice adhesion its 54 kPa. addition, PDA-modified endow with properties. Under irradiation simulated sunlight, rapidly reached 61°C within 3 min, droplets completely melted in 155 s. Besides, it's withstand wide range chemical attacks mechanical impacts. After 15 icing-de-icing cycles 40 sandpaper abrasions test, can still maintain remarkable ice-removal performance, demonstrating robustness stability harsh environments.

Language: Английский

Design and performance evaluation of sunflower straw biochar–based photothermal hydrophobic wood DOI Creative Commons

Siyu Chang,

Lei Wang,

Lihong Yao

et al.

Industrial Crops and Products, Journal Year: 2025, Volume and Issue: 228, P. 120865 - 120865

Published: March 20, 2025

Language: Английский

Citations

0

SiO2/polydopamine photothermal superhydrophobic coating with good anti-icing performance DOI
Yuting Zhong, Yong Liu,

Xiangming Yang

et al.

Surface Engineering, Journal Year: 2024, Volume and Issue: 40(7-8), P. 907 - 916

Published: July 1, 2024

The icing phenomenon has become a safety hazard for the normal operation of equipment. In this work, we report strategy simply obtaining photothermal anti-icing coatings by spraying acrylic resin, polydimethylsiloxane and polydopamine modified SiO 2 particles on steel plate substrate. prepared icephobic AR/PDMS/SiO @PDA composite coating not only excellent superhydrophobicity (WCA = 162°). It also shows good anti- de-icing performances. superhydrophobic surface was able to delay freezing 614 s at −20°C, ice adhesion its 54 kPa. addition, PDA-modified endow with properties. Under irradiation simulated sunlight, rapidly reached 61°C within 3 min, droplets completely melted in 155 s. Besides, it's withstand wide range chemical attacks mechanical impacts. After 15 icing-de-icing cycles 40 sandpaper abrasions test, can still maintain remarkable ice-removal performance, demonstrating robustness stability harsh environments.

Language: Английский

Citations

1